SPIE Advanced Lithography and Patterning Symposium 2022 – day 3

In the morning, the optical and EUV session included two very good talks on EUV pellicles.  Mark van de Kerkhof described ASML’s latest material, a composite made of metal silicide crystals (if I got that right) that performs just a little bit better than the prior polysilicon-based stack.  At almost 92% transmission (one pass), it is a few percent better than the previous best and survives up to 400W source power.  Is it good enough to be adopted in manufacturing?  I’m not sure.  The next talk by Lintec described a 95% transmitting carbon nanotube pellicle, quite a promising result.  Their pellicle is making progress but did not seem manufacturing ready, requiring a bit more time to mature.

In the metrology session, my colleagues Gian Lorusso and Mohamed Zidan from imec gave a pair of good talks on the metrology challenges for measuring very thin resists.  (Full disclosure – I was a coauthor on both papers.)  When the as-coated resist thickness reaches 10 nm, line/space patterns have almost no contrast in a SEM, making measurement of CD and LWR extremely difficult.  Lowering the SEM voltage to 300V, and even lower for some materials, improved things.  It looks like 15 or 20 nm thickness and above is manageable with the right SEM measurement conditions.

I was also very impressed by Nearfield Instruments and their high throughput AFM, described by Cornel Bozdog.  Using four AFM heads running in parallel they could measure 64 0.5micronX0.5micron regions per wafer and get a throughput of 12 wafers per hour.  While I’m sure the typical “your results may vary” caveat applies, it is still an order of magnitude faster than I would have expected.

Quite a few students are attending the conferences this year, and I’ve been able to meet some of them.  Seeing the look of these eager young people, drinking from the firehose of information pouring out in each of the sessions, makes me hopeful for the future of our industry.

SPIE Advanced Lithography and Patterning Symposium 2022 – day 2

The first talk of the metrology conference on Tuesday was by Andras Vladac of NIST on a topic I am very interested in – characterizing the non-ideal behavior of scanning electron microscopes.  His presentation style was somewhat unique:  taking the material from what appeared to be a half-day short course and presenting it in 20 minutes.  This is a definitely a talk where viewing and studying it later (thanks to SPIE’s recording) is a must.  The other talks in the SEM session were good as well, but more digestible.

Tuesday was packed with customer meetings for me – a mixed blessing.  I missed many good talks, but got to have facetime with people I had not been able to visit for at least two years.  I managed to catch the end of Erik Hosler’s plenary talk in the afternoon on “The path to a useful quantum computer”.  One of the more interesting insights was his need to use state-of-the-art immersion lithography for the fabrication of his devices, not for the resolution but for the precision of the manufacturing.  For an optical device, feature sizes are in the hundreds of nanometers or microns.  But quantum optical devices require on the order of 1 nm line-edge roughness from those features, which definitely pushes state-of-the-art capabilities and makes fabrication quite challenging.

SPIE Advanced Lithography and Patterning Symposium 2022 – day 1

As always, the opening of the symposium began with some awards.  Our community’s biggest and most prestigious is the Frits Zernike Award for Microlithography, and it was wonderful to see Harry Levinson receive this year’s honor.  (Full disclosure – I’m on the award selection committee.)  Additionally, since last year’s award ceremony was virtual, Bruce Smith was giving his 2021 Frits Zernike Award for Microlithography as well.  Congratulations to them both!

Four presentations of SPIE fellow were made next:  Nelson Felix of IBM, Kevin Lucas of Synopsys, Uzodinma Okoroanyanwu of the University of Massachusetts, and Tatyana Sizyuk of Argonne National Laboratory.  It’s a shame that Kevin and Uzo could not be here this week.

We next heard two of the three plenary talks (Eric Hosler’s talk on quantum computers will be given on Tuesday.)  The first talk was by Luc Van den hove, President and CEO of imec.

A quick digression.  We have had over the years a number of plenary talks given by various industry executives covering topics of interest to our community such as compute scaling, artificial intelligence, the automotive industry, progress in GPUs, etc.  My biggest fear for these kinds of speakers is getting what I call the “kid on a skateboard” talk.  The executive, giving the same talk they might give at an investor conference, says things like “Technology A is very important” while showing a kid on a skateboard, “Our company is ahead on technology B” then shows a family playing with a dog, etc.  Very slick, and devoid of useful content.  So when a CEO is asked to give a talk on a Wall Street-friendly topic such as “The endless progress of Moore’s Law”, I usually get worried.

But Luc Van den hove is not your typical CEO.  He is a lithographer deep in his bones.  He published his first SPIE paper in 1990, and was chairman of the Optical Microlithography conference in 1998 and 1999.  He knows what he is talking about, and cares deeply about this community.  So when the first few slides in his talk were of the “kid on a skateboard” variety, I was not worried.  He soon got into the technical meat of the topic, and we were all rewarded for our patience.  Taking the broad view of what Moore’s Law means that is typical of today, he described four general areas that will keep progress in semiconductors moving for quite some time (though not the hyperbolic “endless”):  Shrinking the transistor, improving the transistor, moving into the third dimension, and shifting compute paradigms.  I suspect that he is correct on all counts.

The second plenary by H.S. Philip Wong of Stanford went into considerably more detail on two of Luc’s topics, system-level optimization and 3D integration.  Dr. Wong is an expert on these topics and I learned quite a bit.  He would have been better off, however, if he had not tried to force lithography relevance into his talk through his provocative title and subsequent discussion of EUV lithography throughput (Tony Yen – you were a bad influence!).

For the rest of the day I alternated between the metrology conference and the two keynote talks at the Optical and EUV Nanolithography conference.  Nelson Felix gave a nice review of metrology needs for nanosheet transistors, though I was very surprised when he showed that 1/3 of all the process steps in IBM’s latest generation process were metrology steps, and that this hasn’t changed since the 45 nm node.  There is no doubt that IBM does more metrology than your typical fab.  Mark Phillips of Intel gave a very optimistic view of when high-NA EUV lithography could be inserted into manufacturing, beating by a year the roadmap shown by Luc Van den hove (which, coming from imec, could also be assumed to be optimistic).  It sounds to me that Intel is tired of being behind in EUV and is hoping that high-NA EUV will give them a chance to leapfrog ahead.

I ended the day with a Fractilia hospitality event at a favorite San Jose brew pub.  Thanks to all who joined us!

SPIE Advanced Lithography and Patterning Symposium 2022 – day 0

“The SPIE Advanced Lithography conference begins with one word on everyone’s mind:  coronavirus.”  These are the first words I used in my blog post two years ago, just as the SPIE Advanced Lithography Symposium of 2020 was about to begin on February 23.  I had no way of knowing that within three weeks pretty much the whole country would start locking down.  That 2020 conference went off without any known coronavirus transmissions, thank goodness, and two+ years later I think that first sentence applies equally well today.  Last year’s symposium was virtual, and this year’s has been postponed two months, just long enough to allow the Omicron variant to fad and for most of us to gather with more confidence.

It’s good to be live and in-person!  I’ve already seen on Sunday several folks that I have only seen on Zoom for the last two years, and it is a great pleasure!  The conference is promising to be a good one, effected though it is by the lingering impact of the pandemic.  Virtually no one from Taiwan, Korea, or Japan has been able to attend, and participation from Europe is down significantly.  Still, registration currently sits at 1,300 (as opposed to the pre-pandemic average of about 2,000), which is better than I was expecting.  There were 390 paper submissions this year (in 2020, the number was about 500) and I’m hoping for a very good program.

There have been a couple of major changes in the symposium this year.  The EUV and Optical Lithography conferences have merged (now called Optical and EUV Nanolithography), reflecting the continued mainstreaming of EUV lithography out of development and into semiconductor manufacturing.  The topic of computational lithography, formerly homed in the Optical Lithography conference, now resides in the refocused DTCO and Computational Patterning conference.  These are both good changes, and I look forward to seeing how they play out this week.

Does a mirror invert an image left-to-right?

A recent query from a friend reminded me that some topics are both very easy and very hard to grasp at the same time. The key is often in the way we look at the it. He asked “Why does a mirror NOT invert images top-to-bottom?”  Or better yet, why DOES a mirror invert images left-to-right? I used to ask this question to my undergraduate students in my Modern Optics class at UT when teaching them basic imaging equations. None of them ever answered the question correctly. But the answer, it turns out, is simple.   Mirrors don’t invert anything.  You do, and not with your brain.

Try this experiment.  Go up to a mirror with an open book in your hand.  Look at the printing – obviously it is perfectly readable.  Now turn the book to face the mirror – you see that all of the writing in the mirror is inverted, going from right to left instead of left to right.  What caused that?  You did, when you TURNED the book.  Don’t believe me?  Repeat the experiment with an overhead transparency (yes, I am old enough to know what those are).  Write a word on the overhead transparency and hold it up to the mirror.  It is not inverted, when looking at it either directly or in the mirror.  When you turn the transparency to face the mirror, the word is inverted when viewed both directly and in the mirror.

When you look at yourself in the mirror and wave your right hand, it looks like your mirror image is waving their left hand. But that is because we imagine ourselves turned around and facing the other way. Again, it the turning (or imaging that we turned) that does the inverting, not the mirror.

Mystery solved.

SPIE Advanced Lithography Symposium 2021 – day 5

One advantage of the all-online format of this year’s symposium is that the conference can be stretched from the normal four days to five without significant cost impact.  This means that several ‘live” events were spread out through Friday, including several very good keynote talks and a second tutorial talk.  Jara Garcia Santaclara of ASML spoke on resist development for high-NA EUV lithography.  (Jara has what I think is the world’s best job title:  EUV Resist & Processing Architect.  I love it!)  One of the biggest concerns for high-NA EUV imaging is the need for a much thinner resist (20 nm, maybe less), with numerous consequences stemming from that fact.  Metal-containing resists are the leading candidates here, since their higher absorption enables thinner resist films.  This nice overview talk led well into the second Patterning Materials keynote by Rich Wise of Lam Research.  A year ago, Rich introduced a new resist offering by Lam based on a dry-deposited, dry-developed metal-based material that they developed.  The early results a year ago looked promising, and the updated results this year look really good.  They have made a lot of progress in one year!  Could it be that Lam will beat the industry track record of requiring at least one decade to introduce a new resist platform?  It looks like Inpria has some competition.

Regina Freed of AMAT gave a nice keynote on etching.  I especially liked learning about some of the unique challenges of DRAM manufacturing.  The day ended with a very well-done tutorial talk about lithography’s endgame by Ralph Dammel.  After a resist-focused history of wavelength transitions (Ralph is a consummate resist chemist, after all), he suggests (perfectly correctly, in my opinion) that 13.5 nm will be our last wavelength.  This means that the end of lithography-based scaling is near, and non-scaling-based innovations in chip making (in particular, vertical scaling) will enable a continuation of Moore’s Law in a new way.  I couldn’t agree more, though I would add that alternate chip architectures, new materials enabling new types of chip components, and innovations in chip design will probably keep Moore’s Law going for quite a while as well.

All-in-all, this digital forum for Advanced Lithography went better than I expected.  Still, I’m looking forward to next year’s in-person version, perhaps with some of the best practices of this year’s version blended in.  We shall see.

SPIE Advanced Lithography Symposium 2021 – days 3&4

On Wednesday and Thursday there were several live events, and I went through many, many prerecorded talks.  There were three metrology keynotes.  The Samsung talk (on Tuesday, but I watched it later) was a broad overview of the challenges for metrology in the semiconductor industry (summary:  its challenging).  The KLA and Applied Material keynotes, while containing some interesting information, were mostly marketing presentations – not my favorite style for this conference.  The Novel Patterning keynote was given by a former lithographer that I was happy to see back at this conference – Mike Fritze, now at a Washington think tank.  He talked about the market for low-volume IC manufacturing, now dominated by the use of used equipment.  Since Moore’s Law scaling has dramatically slowed and will slow even more in the coming years, and since the latest generation of tools may be too expensive to operate at any time for anyone but the biggest volume fabs, will there be a market for special-built lithography tools (such as direct-write) to serve the long-term needs of a growing ASIC (application -specific integrated circuit) market?  Mike raised interesting questions, provided interesting speculations, and presented historical data in useful ways – a great talk.

Mike’s talk was interesting to watch just before Donis Flagello’s Optical Lithography keynote.  More than 10 years ago Nikon ceded the next-generation lithography landscape to ASML, then also lost considerable market share in 193-immersion tools.  What is Nikon’s growth strategy in lithography?  Donis showed us that it is mostly emerging new markets, either outside the semiconductor market or niches within the semiconductor industry.  Nikon has been working on an optical direct-write tool for some time (the so-called Digital Scanner), but also is getting into 3D manufacturing with a tool for additive and subtractive direct metal processing for both macroscopic and microscopic patterning.  The most interesting idea, for this community anyway, was a concept for a two-beam EUV imaging tool.  A combination of a grating phase mask and one-direction wafer scanning could produce sub-30nm pitch lines and spaces over an entire wafer.  The simplified optical design would have much higher optical transmission, enabling good throughput with only moderately ridiculous EUV sources.  At least in concept.  We shall see if Nikon will invest the HUGE amount of money it would take to bring a tool like this to market.

I presented what was called a live “tutorial and networking event”.  The topic was how to use the power spectral density to understand roughness (a prerecorded talk), and what made it a networking event was that viewers could turn on their cameras at the end and ask me questions directly, rather than through the Q&A feature of Zoom and relayed by the moderator.  I liked that format, and was surprised to find out that 20+ minutes for Q&A was not enough!  The second such event will be on Friday with Ralph Dammel, which I am very much looking forward to.

I attend both poster sessions for about 30 minutes each.  The same posters were available in each, and the two sessions (one morning, one late afternoon) were intended to enable Europe and Asia to participate in at least one.  They were very disappointing.  It is not because the software platform (Remo) did not work well – I actually liked it.  Each poster was set up at a virtual table, and attendees could move to any table, view the poster (as a “white board” that anyone at the table could point to), and interact with others at the table if they wanted.  This worked pretty well.  The problem was that very few of the poster authors actually showed up.  We can view the pasters any time we want on the digital library, so the whole point of the live poster session was to interact with authors.  None of the authors I wanted to talk to were there on either day.

There were a slew of good papers that I watched.  Jan Van Schoot gave a great overview of ASML’s progress on their high-NA EUV system (which was considerable).  Still, I find their timetable on deployment terribly optimistic, even given ASML’s considerable tool development prowess.  Eric Verhoeven described the NXE:3600 due out this summer, another useful and needed incremental advance of the core NA=0.33 EUV system.  Since the 250W sources have been out in the field for a while, and by all accounts working well, everyone is looking towards the next source power advance, possibly as high as 500W. 

There were many papers on EUV stochastic defectivity (a particular interest of mine).  So here is some blatant self-promotion.  Danilo De Simone in his talk on 28nm pitch single patterning with EUV showed CD and unbiased linewidth roughness measurements using MetroLER and said “There is a correlation between defectivity and roughness. This is also an important point to mention.”  The reason it is important is that roughness is easy to measure (with tens or hundreds of SEM images), but defectivity for a good process may require many thousands or millions of SEM images.  I authored or coauthored three papers this year, all of which I will claim are useful contributions to the field of stochastic measurements and their use (but I am biased, even if my measurements are not).  The paper by IBM that I coauthored (I only helped with some of the measurements) showed yet another example of how biased roughness measurements can produce incorrect trends and decisions as compared to unbiased measurements.

Have you ever heard of the Kullback-Leibler divergence?  Neither had I, but thanks to a paper by Zachary Levinson of Synopsys, I’m going to look it up.  Luke Long of UC Berkeley contributed nice simulation work on the impact of diffusion, development, and etch to the 3D mechanism of missing contact holes.  I also watched several good etch/patterning papers (helping to reduce, ever so slightly, my knowledge gap on that topic), covering selective deposition and atomic layer etch/deposition cycles.  These approaches can produce aspect-ratio dependent results, which enable healing of stochastic variations of line/spaces or contact holes.  Fascinating.  Nayoung Bae of TEL taught me about DRAM contact hole staggered array formation using crossed SADP or SAQP lines, and the multiple populations of holes that result.  Characterizing the stochastics of the lines and spaces helps to understand the LCDU of the resulting holes.

It was good, busy, and technically packed couple of days.  I’m looking forward to the final live events of Friday as the conference wraps up.

SPIE Advanced Lithography Symposium 2021 – day 2

Attending a virtual conference is obviously much different than in-person.  When it comes to Advanced Lithography, one of the biggest differences is the lack of parallel sessions.  A typical Tuesday at the San Jose Convention Center would involve dashing between sessions to catch talks, sometimes cursing that the two talks I wanted to see most were at the same time, and sometimes realizing that there are no talks I want to see for the next two hours.  There is a lot of “task switching”, where my mind alternates among the physics of shot noise, the chemistry of resist development, and the usefulness of the latest metrology tool advance.  This week on Tuesday, I binge-watched all the metrology talks (or rather, the 50% or so of them I was most interested in).  It was both fun and exhausting.

As one might expect, the highlights for me were the topics that most closely related to my work.  I watched the presentations on the latest SEM tools, though there was essentially nothing related to the physics of SEM image formation, my special interest.  There were many papers on how to employ SEM contours in metrology use cases rather than just traditional CD values, a topic that I have been seeing at this conference for 25 years.  It seems we have still not solved all the many issued required to make that happen.  Yosuke Okamoto’s talk helps explain why – contours can change significantly depending on the scan direction of the CD-SEM.

Of course, there were many papers on roughness measurement, with most of them related to machine learning in some way.  I have to admit that I am not a big fan of image denoising.  Maybe I’m just an old guy who prefers understanding the physics rather than letting a neural network make connections we can never understand.  I also think that many people working on image denoising are not carefully defining metrics of success that a metrologist would appreciate, things like accuracy and precision, repeatability and the size of the error bars around your answer.  Getting an image that looks less noisy is not success.

I liked George Orji’s talk on wavelet analysis of roughness.  Someday I’ll have to do the work to really understand wavelets, beyond the surface level I have today.  My hat’s off to George Papavieros for trying to measure LER with a SEM pixel size (in the direction perpendicular to the line edge) that is greater than the 3sigma LER.  That is not something I want to try.  I am a big fan of the stochastic process window (something that both Fractilia and ASML have been promoting lately), and there were a few ASML talks with some interesting results.  In a stochastic process window, one includes stochastics measures (such as defectivity, LCDU, or unbiased LWR) in the focus-exposure process window determination in addition to CD.  From Mary Breton’s talk I got a good sense of the nanosheet gate fabrication process and what metrology needs exist at each step.

I also watched the EUV conference keynote, a “live” event on Zoom.  Jos Benschop gave a very nice (prerecorded) talked, followed by live Q&A.  And sure enough, it was the Q&A that was the most interesting part.  I also will have a live event Wednesday afternoon (3pm Pacific Time), a tutorial and networking event.  This is a new presentation format for this conference, so we are all anxious to see how it will go.  The 35-minute prerecorded tutorial on the power spectral density will be followed by 25 minutes for Q&A and networking.

With my metrology binge-watching over, it is time to move on to the other conferences as the next day begins.

SPIE Advanced Lithography Symposium 2021 – day 1

As with the in-person version of this symposium, AL21 began Monday morning with an opening session and two of the three plenary talks.  This was a “live” event, though I think a recording of it will show up in the SPIE Digital Library soon.  The first item of business was the awarding of new SPIE Fellows in the lithography community.  Congratulations to Yi-sha Ku of ITRI in Taiwan, Anna Lio of Intel, John Robinson of KLA, and Mark Somervell of TEL for becoming fellows this year.  The Frits Zernike Microlithography Award went to Bruce Smith of RIT – congratulations for this well-deserved honor.  It is also a bit overdue, due to Bruce’s long-time service as the chair of the Zernike Award committee, which made him ineligible until he left that post.

The Nick Cobb Memorial Scholarship went to Yuka Esashi of the University of Colorado Boulder, who is working on her PhD in Physics on the topic of EUV reflectometry.  I had a chance to talk to Yuka during a virtual student networking event later that evening and I suspect she will be much sought after in the semiconductor industry when she graduates in a couple of years.

After the loss of one of the greats from our community, Bill Arnold, it was appropriate that his friend and colleague Mircea Dusa gave a nice overview of his contributions to our industry and a series of remembrances about his life.  Thank you, Mircea.  Bill will be missed.

The opening remarks ended with an overview of the changes that will come to this symposium next year.  First, the name of the symposium will change from Advanced Lithography (AL) to Advanced Lithography and Patterning to reflect the continued integration of lithography with deposition, etch, and other processes to produce complex patterns.  The biggest change will be the merging of the optical and EUV lithography conferences into the “Optical/EUV Nanolithography and Practices” conference, reflecting the emergence of EUV as a manufacturing technology.  The computational lithography pieces of the old Optical Lithography conference will now go to the renamed “DTCO and Computational Patterning” conference.  There have also been a few smaller changes to the scopes and names of the other conferences.  The result will be a symposium with six conferences next year, rather than the seven we have this year.

As Michael Mayberry of Intel began his plenary talk, I quickly realized one of the major downsides of a virtual conference.  It seems that none of my regular work meetings for the week have been cancelled.  How did that happen?  I had to leave Mike’s talk just as he was getting started.  Eventually, I believe that this plenary will be available on the SPIE Digital Library so I can finish watching it, but not yet.

I did see John Hu of NVIDIA give his plenary on trends in high performance computing.  While I enjoyed the talk in general, I have two specific complaints that can’t go unmentioned.  First, as an example of the power of GPU rendering he showed a clip of a digital supermodel walking around in a bathing suit.  This is obviously inappropriate for a technical conference, especially one in a male-dominated industry like ours.  Second, at the end of his talk, he described the goal to “create a virtual world better than real”.  Really?  First of all, I don’t think that could ever happen.  But if it ever did that only means we should stop working on creating better virtual worlds and focus on improving the real one.  Time to pick a better goal.

I also began the process of working my way through the many interesting technical talks (viewable on demand).  I’ll have more to say about what I am learning from them in a subsequent post, but let’s just say I’m a fan of 1.5X speed.

SPIE Advanced Lithography Symposium 2021 – prologue

Beginning in 2006, I have blogged each year at the SPIE Advanced Lithography Symposium, the major event of the year in the field of lithography and patterning.  Each morning of the conference I would wake up very early and write a post about my impressions from the day before.  (A complete collection of these “conference diaries” can be found here.)  I have always enjoyed the process of writing, and even more enjoyed the reactions these posts got.  Numerous people, unable to attend, would following along with my posts and capture just a small sense of what this fantastic event was all about.  Putting my thoughts into words has always been clarifying for me, with the added benefit of helping me organize the massive amount of information that was flooding over me, with the hope that some if that knowledge might stick.

This blogging tradition is just one more casualty of the crazy pandemic year.  At last year’s conference we were all talking about Covid, using hand sanitizer, and wondering whether it would actually turn into a pandemic.  I think, in hindsight, we were very lucky that the 2,000 attendees had no known transmissions during the conference.  Within two weeks of the end of AL 2020 much of the country began shutting down.

And now it is one year later.  An in-person conference is out of the question.  Instead, SPIE has created a “Digital Forum” for AL 2021.  There will be a few “live” events sprinkled throughout the week, but all of the technical talks have been prerecorded and are available for viewing at any time during the week to conference “attendees”.  The registration fee for the conference is about half the cost for attending in-person last year.  The first live event will be the conference kick-off on Monday (8am pacific time).

Of course, I will miss being there in person, seeing old friends and making new ones, talking in the hallways, drinking too much coffee in the mornings and beer in the evenings, laughing and learning, even doing a little business on the side.  I will miss seeing the audience when I give a talk.  I will miss approaching the microphone to ask a question after listening to someone else’s talk.  But given our current reality, I am looking forward to attending this week’s on-line events and binge-watching technical talks.  I’ll take advantage of the unique benefits of asynchronous viewing, slowing down or speeding up the flow of information to my needs and desires.  It won’t be perfect, but I think it will be good.  Let the Digital Forum begin!

Musings of a Gentleman Scientist